SURFACE | CHARACTERISTIC | SUMMARY OFMANUFACTURING METHOD | APPLICATION |
NO.1 | Silvery white | Hot rolled to specified thickness | Do not need to have a glossy surface use |
| Lackluster |
|
|
NO.2D | Silvery white | After cold rolling, heat treatment and pickling are carried out | General material,deep material |
NO.2B | Gloss is stronger than NO.2D | After NO.2D treatment,the final light cold rolling is carried out through the polishing roller | The general material |
BA | As bright as a sixpence | No standard,but usually a bright annealed surface with high reflectivity | Building materials,kitchen utensils |
NO.3 | Rough lapping | Grind with 100-200#(unit)strop tape | Building materials,kitchen utensils |
NO.4 | Intermediate grinding | Polished surface obtained bygrinding with150~ 180# strop abrasive tape | Building materials,kitchen utensils |
NO.240 | Fine lapping | Grinding with 240# strop abrasive tape | Kitchenware |
NO.400 | The luster is close to BA | Use 400# polishing wheel to grind | General,timber,building,timber,kitchen appliances |
HL | Hairline grinding | Suitable particle material for hair stripe grinding(150~240#)with many grains | Building.construction material |
NO.7 | It s close to mirror grinding | Use a 600# rotary polishing wheel to grind | For art or decoration |
NO.8 | Mirror ultra finish | The mirror is ground with a polishing wheel | Reflector,for decoration |